... cylinders, welded together endwise. Each ring was made of bars wound upon an arbor spirally, like winding a ribbon upon a block, and, being welded and shaped in dies, were joined endwise, when in the furnace and at a welding heat, and afterwards pressed... Proceedings of the American Academy of Arts and Sciences - Stran 38avtor: American Academy of Arts and Sciences - 1868Celotni ogled - O knjigi
| American Academy of Arts and Sciences - 1857 - 532 strani
...furnace and at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1,000 tons' force. Finding in the early stage of the manufacture...previously formed steel ring. Eight of these guns were 6-pgunders of the common United States bronze pattern, and eleven were 32-pounders of about 80 inches'... | |
| 1857 - 426 strani
...furnace and at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1,000 tons' force. Finding in the early stage of the manufacture...those made afterwards with a lining of steel, the wrought iron bars being wound upon a previously formed steel ring. Eight of these guns were 6-pounders... | |
| 1857 - 424 strani
...furnace and at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1,000 tons' force. Finding in the early stage of the manufacture...those made afterwards with a lining of steel, the wrought iron bars being wound upon a previously formed steel ring. Eight of these guns were 6-pounders... | |
| 1857 - 424 strani
...furnace and at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1,000 tons' force. Finding in the early stage of the manufacture that the softness of the wrought iron was a serions defect, I formed those made afterwards with a lining of steel, the wrought iron bars being... | |
| Andrew Ure - 1860 - 972 strani
...furnace and at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1000 tons force." Finding in the early stage of the manufacture...softness of the wrought iron was a serious defect, he formed those made afterwards with a lining of steel, the wrought-iron bars being wound upon a previously... | |
| 1866 - 460 strani
...furnace at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1000 tons' force. Finding in the early stage of the manufacture...those made afterwards with a lining of steel, the wrought iron bars being wound upon a previously formed steel ring. Eight of these guns were 6-pounders... | |
| 1867 - 400 strani
...in the early stage of the manufacture that the softness of the wrought-iron was a serious defect, 1 formed those made afterwards with a lining of steel,...wound upon a previously formed steel ring. Eight of theseguns were six-pounders, of the common United States bronze pattern, and eleven were thirty-two-pounders,... | |
| Andrew Ure - 1867 - 1006 strani
...furnace and at a welding heat, and afterwards pressed together in a mould by a hydrostatic press of 100O tons force." Finding in the early stage of the manufacture...softness of the wrought iron was a serious defect, he formed those made afterwards with a lining of steel, the wrought-iron bars being wound upon a previously... | |
| 1857 - 426 strani
...and at a •welding heat, and afterwards pressed together in a mould by a hydrostatic press of 1,000 tons' force. Finding in the early stage of the manufacture...those made afterwards with a lining of steel, the wrought iron bars being -wound upon a previously formed steel ring. Eight of these guns were 6-pounders... | |
| 1873 - 800 strani
...iron was a serious defect, I formed those made afterwards with a lining of steel, the wrought iron bars being wound upon a previously formed steel ring. Eight of these guns were 6-pounders of the common United States bronze pattern, and eleven were 32-pounders, about eighty inches... | |
| |